This paper deals with the use of industrial by-products from electric arc furnace (EAF) granulated slag for the partial replacement of natural aggregates commonly used to manufacture concrete. Three different gradings of EAF granulated slag were considered. The rheological and mechanical properties of concrete manufactured with a partial replacement of natural aggregates with slag were determined. Dry shrinkage of hardened concrete was evaluated. Results indicated that the maximum percentage of natural aggregate that can be replaced with EAF granulated slag is about 15% in order to limit the superplasticizer dosage required to attain the same workability class of the reference concrete mix at the end of the mixing procedure. The higher the percentage of granulated slag was, the higher the density, the elastic modulus in compression and the compressive strength of the concrete were. Dry shrinkage of the concrete increased by adding a greater amount of EAF granulated slag.
(2016). Electric arc furnace granulated slag for sustainable concrete [journal article - articolo]. In CONSTRUCTION AND BUILDING MATERIALS. Retrieved from http://hdl.handle.net/10446/72932
Electric arc furnace granulated slag for sustainable concrete
COPPOLA, Luigi;BUOSO, Alessandra;COFFETTI, Denny;LORENZI, Sergio
2016-01-01
Abstract
This paper deals with the use of industrial by-products from electric arc furnace (EAF) granulated slag for the partial replacement of natural aggregates commonly used to manufacture concrete. Three different gradings of EAF granulated slag were considered. The rheological and mechanical properties of concrete manufactured with a partial replacement of natural aggregates with slag were determined. Dry shrinkage of hardened concrete was evaluated. Results indicated that the maximum percentage of natural aggregate that can be replaced with EAF granulated slag is about 15% in order to limit the superplasticizer dosage required to attain the same workability class of the reference concrete mix at the end of the mixing procedure. The higher the percentage of granulated slag was, the higher the density, the elastic modulus in compression and the compressive strength of the concrete were. Dry shrinkage of the concrete increased by adding a greater amount of EAF granulated slag.File | Dimensione del file | Formato | |
---|---|---|---|
Coppola et al_EAF slag for sustainable concrete_CBM.pdf
Open Access dal 02/10/2018
Versione:
postprint - versione referata/accettata senza referaggio
Licenza:
Creative commons
Dimensione del file
759.02 kB
Formato
Adobe PDF
|
759.02 kB | Adobe PDF | Visualizza/Apri |
j.conbuildmat.2016.06.142.pdf
Solo gestori di archivio
Versione:
publisher's version - versione editoriale
Licenza:
Licenza default Aisberg
Dimensione del file
637.91 kB
Formato
Adobe PDF
|
637.91 kB | Adobe PDF | Visualizza/Apri |
Pubblicazioni consigliate
Aisberg ©2008 Servizi bibliotecari, Università degli studi di Bergamo | Terms of use/Condizioni di utilizzo