This paper is aimed to study the rheological and physical performance of mortars manufactured replacing Portland-based cements with low calcium siliceous fly ash (FA) or ultrafine fly ash (UFFA). Five different types of cement (CEM I, CEM II/A-LL, CEM III/A, CEM III/B, and CEM IV according to EN 197-1) were used. Mortars were manufactured with FA or UFFA replacing 5%, 15%, 25%, 35%, and 50% of cement mass. Results indicate that compressive strength of mortars with UFFA is considerably higher than that of mixtures containing traditional FA, both at early and long ages. Moreover, experimental data reveal that replacement of cement with up to 25% of UFFA determines higher compressive strength at 7, 28, and 84 days than plain mortars (containing cement only), regardless of the type of cement used. Mortars manufactured with 35% or 50% of UFFA show slightly lower or similar compressive strength compared to the reference mortar (containing cement only). In addition, the results show values of the strength activity index of mortars made with FA 25%, 23%, and 20% lower than the reference corresponding mortars (cement only) at 7, 28, and 84 days, respectively. The grinding of FA, despite resulting in an increase in production energy and CO2emissions compared to unmilled FA, allows a wide use of these SCM (Supplementary Cementitious Materials) in place of cement, reducing the environmental impact of mortars up to 40% at the 28-day strength class. The use of UFFA ensures better resistance in CaCl2-rich environments.
(2018). Plain and ultrafine fly ashes mortars for environmentally friendly construction materials [journal article - articolo]. In SUSTAINABILITY. Retrieved from http://hdl.handle.net/10446/130873
Plain and ultrafine fly ashes mortars for environmentally friendly construction materials
Coppola, Luigi;Coffetti, Denny;Crotti, Elena
2018-01-01
Abstract
This paper is aimed to study the rheological and physical performance of mortars manufactured replacing Portland-based cements with low calcium siliceous fly ash (FA) or ultrafine fly ash (UFFA). Five different types of cement (CEM I, CEM II/A-LL, CEM III/A, CEM III/B, and CEM IV according to EN 197-1) were used. Mortars were manufactured with FA or UFFA replacing 5%, 15%, 25%, 35%, and 50% of cement mass. Results indicate that compressive strength of mortars with UFFA is considerably higher than that of mixtures containing traditional FA, both at early and long ages. Moreover, experimental data reveal that replacement of cement with up to 25% of UFFA determines higher compressive strength at 7, 28, and 84 days than plain mortars (containing cement only), regardless of the type of cement used. Mortars manufactured with 35% or 50% of UFFA show slightly lower or similar compressive strength compared to the reference mortar (containing cement only). In addition, the results show values of the strength activity index of mortars made with FA 25%, 23%, and 20% lower than the reference corresponding mortars (cement only) at 7, 28, and 84 days, respectively. The grinding of FA, despite resulting in an increase in production energy and CO2emissions compared to unmilled FA, allows a wide use of these SCM (Supplementary Cementitious Materials) in place of cement, reducing the environmental impact of mortars up to 40% at the 28-day strength class. The use of UFFA ensures better resistance in CaCl2-rich environments.File | Dimensione del file | Formato | |
---|---|---|---|
Plain and Ultrafine Fly Ashes Mortars for.pdf
accesso aperto
Versione:
publisher's version - versione editoriale
Licenza:
Creative commons
Dimensione del file
4.2 MB
Formato
Adobe PDF
|
4.2 MB | Adobe PDF | Visualizza/Apri |
Pubblicazioni consigliate
Aisberg ©2008 Servizi bibliotecari, Università degli studi di Bergamo | Terms of use/Condizioni di utilizzo